Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON™ A-TECH™ 1170 - (PS-HI) - Americas Styrenics LLC

Material Data Center offers the following functions for STYRON™ A-TECH™ 1170:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Styron A-Tech datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 1.9 g/10min ASTM D 1238
Temperature 200 °C -
Load 5 kg -
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 1379 MPa ASTM D 638
Tensile Strength 22.1 MPa ASTM D 638
Tensile Strength at Break 29 MPa ASTM D 638
Flexural Modulus 1448 MPa ASTM D 790
Flexural Strength 31.7 MPa ASTM D 790
Rockwell Hardness R 103 - ASTM D 785
Izod Impact notched, 1/8 in 90.7 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
Coefficient of Thermal Expansion, MD 90 E-6/K ASTM D 696
DTUL @ 66 psi 90.6 °C ASTM D 648
DTUL @ 264 psi 79.4 °C ASTM D 648
Vicat Temperature 104 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 1040 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Mold temperature 17 - 65 °C -
Zone 1 218 - 249 °C -
Zone 2 218 - 249 °C -
Zone 3 199 - 213 °C -
Nozzle temperature 213 - 243 °C -
Back pressure 0.172 - 1.21 MPa -
Processing Recommendation ExtrusionValueUnitTest Standard
Melt temperature 193 - 232 °C -
Zone 1 177 - 193 °C -
Zone 2 182 - 204 °C -
Zone 3 188 - 210 °C -
Zone 4 199 - 216 °C -
Zone 5 204 - 221 °C -
Nozzle temperature 199 - 232 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Special Characteristics
High impact or impact modified
Features
Color Stability
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Refrigeration
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.